Effect of Ash Pozzolan on the Physical and Mechanical Properties of Wood Cement Composites
Effect of Ash Pozzolan on the Physical and Mechanical Properties of Wood Cement Composites
Mona Shayestehkia1 Amir Hooman Hemmasi2 Hossein Rangavar3
1) 1. PhD, Department of Wood and Paper Science and Technology, Faculty of Natural Resources and Environment, Science and Research Branch, Islamic Azad University, Tehran, Iran , e-mail address
2) 2. Professor, Department of Wood and Paper Science and Technology, Faculty of Natural Resources and Environment, Science and Research Branch, Islamic Azad University, Tehran, Iran
3) 3. Associate Professor, Department of Wood and Paper Industries, Shahid Rajaee Teacher Training University, Tehran, Iran.
IOI Code
:
ABKD-ACZKGF
Publication :
Fourth International Conference on applied researches in civil engineering, architecture and urban planning (icarcau.com)
Abstract :
This study examined the effects of ash pozzolan and calcium chloride on the physical and mechanical properties of wood cement composites. Boards were made from pine wood flour at cement to wood flour ratios of 3 and 4 (wood-to-cement ratios of 1:3 and 1:4), with pozzolan at 0, 10 and 20% and calcium chloride as an accelerator at 6 and 8%. Modulus of elasticity (MOE), modulus of rupture (MOR), internal bond strength (IB), water absorption (WA) and thickness swelling (TS) were measured and analyzed by analysis of variance and Duncan’s test. On average, MOE, MOR and IB increased with higher pozzolan and calcium chloride contents, and a higher cement ratio increased MOE and MOR (the main effect of cement ratio on IB was not significant). The highest MOR (51.07 MPa) and IB (0.96 MPa) were obtained with a cement ratio of 4, 8% calcium chloride and 20% pozzolan. The highest MOE (2.67 GPa) was obtained with 6% calcium chloride at the same ratio and pozzolan level, but it did not differ significantly from that of the 8% treatment (2.66 GPa). The lowest MOE, MOR and IB occurred at a ratio of 3 with 6% calcium chloride and no pozzolan. TS decreased with higher pozzolan content, calcium chloride content and cement ratio, whereas WA decreased significantly only with higher pozzolan content. The lowest mean TS (5.22%) was found at a ratio of 4 with 8% calcium chloride and 20% pozzolan, and the highest (9.48%) at a ratio of 3 with 6% calcium chloride and no pozzolan.