Physical and mechanical strength evaluation of self-leveling mortar with polypropylene fibers and silica aggregates
Physical and mechanical strength evaluation of self-leveling mortar with polypropylene fibers and silica aggregates
Ali Sahraei1 Hamid Beiraghi2
1) Department of Civil Engineering, Mahdishahr Branch, Islamic Azad University, Mahdishahr, Iran -
2) Department of Civil Engineering, Mahdishahr Branch, Islamic Azad University, Mahdishahr, Iran -
IOI Code
:
AACC-AAKFFB
Publication :
Third International Conference on applied researches in civil engineering, architecture and urban planning (icarcau.com/3rd)
Abstract :
In this study, self-leveling mortars based on Portland cement type 2 are examined.
First, the history and necessity of using self-leveling mortars are reviewed, then the properties of the constituent materials are introduced. Considering that in self-leveling mortars that have been previously used by various individuals and companies, the maximum compressive strength recorded is between 20 and 55 MPa, and in the first stage, the compressive strength must be increased to at least 90 MPa, and then the laboratory program of fresh and hardened properties, numerical tables, and graphs must be drawn. In this study, sample mixing designs were used in which the amount of microsilica with 5.5, 8, 9, 10, and 12% by weight is replaced by silica aggregates to evaluate the effect of the amount of microsilica on compressive strength and water permeability and other tests. Metakaolin with a weight of 0, 2.5, and 5% by weight is replaced by aggregates, superplasticizer with 0.7, 0.9, and 1.1% by weight, silica aggregates, polypropylene fibers 0.0025, 0.005, and 0.007 volumetric mass of one cubic meter of self-leveling mortar was used. And the defoamer with the values (0, 0.2, 0.4, 0.6, 0.8 and 1% of the total weight) has been presented in the compressive strength test, tensile strength, water absorption rate, and flow test, and the results have been described and explained.
In the results obtained, the use of microsilica and the use of antifoam and superplasticizer and silica aggregates in appropriate proportions increases the 28-day compressive strength to 90 MPa.
Keywords : self leveling mortar microsilica silica aggregate polypropylene fibers and compressive strength tensile strength water absorption fluidity test of self leveling mortar