Simultaneous Effects of Reheating Temperature and Rolling Speed on the Microstructure and Mechanical Properties of Hot-Rolled Products

Simultaneous Effects of Reheating Temperature and Rolling Speed on the Microstructure and Mechanical Properties of Hot-Rolled Products

Amin Gholamalitabar1 Mostafa hekmatpoor2

1) Quality Control Engineer, Arman Asia Steel Melting Company
2) Quality Control Manager, Arman Asia Steel Melting Company

IOI Code : AAHE-ABADHA
Publication : National Conference on Civil Engineering, Design and Construction Technologies, Energy, Materials and Advanced Machinery(icaeu.ir)
Abstract :
    In the hot rolling process of steel, reheating temperature and rolling speed are considered key kinetic and mechanical parameters that play a decisive role in microstructural evolution and the mechanical performance of the final product. The reheating temperature not only controls the initial austenite grain size, but also influences the nucleation rate of recrystallization, grain growth behavior, and the amount of deformation-induced stored energy. In contrast, rolling speed governs the effective strain rate, energy distribution, and the available time for dynamic reactions to occur. An increase in reheating temperature promotes grain growth and reduces the density of active grain boundaries, which may lead to a decrease in strength, whereas higher rolling speeds increase strain rate and dislocation storage, potentially accelerating dynamic recrystallization or, if insufficient time is available, resulting in microstructural heterogeneity. In this study, the combined effects of three reheating temperatures (1050 °C, 1150 °C, and 1250 °C) and three rolling speeds (7, 8.5, and 10 m/s) on the microstructure and mechanical properties of hot-rolled steel were investigated, including grain size, microstructural distribution, yield strength, ultimate tensile strength, elongation, and flexural strength. The results demonstrated that the combination of a reheating temperature of 1150 °C and a rolling speed of 8.5 m/s led to a more uniform microstructure and a well-balanced set of mechanical properties, whereas excessive reheating temperature and rolling speed resulted in coarse-grained and heterogeneous microstructures, adversely affecting toughness and ductility.