Evaluation of Mechanical Properties Fiber Concrete Containing Glass Powder and basalt Powder Exposed to Elevated Temperatures
Evaluation of Mechanical Properties Fiber Concrete Containing Glass Powder and basalt Powder Exposed to Elevated Temperatures
Amirhosein Ehteshami Aziz abad1 Mohsen Falahatkar Gashti2 Mohammad Fard Samimi3
1) Master s student in Structural Engineering, Civil Engineering Department, Rasht Jihad Daneshgahi Institute of Higher Education
2) Assistant Professor, Department of Civil Engineering, Rasht Jihad Daneshgahi Institute of Higher Education
3) Assistant Professor, Department of Civil Engineering, Rasht Jihad Daneshgahi Institute of Higher Education
IOI Code
:
AAHE-ACZBGF
Publication :
National Conference on Civil Engineering, Design and Construction Technologies, Energy, Materials and Advanced Machinery(icaeu.ir)
Abstract :
With the increase in high-rise and strategic concrete structures, maintaining the appearance and mechanical properties of concrete against high temperatures has become one of the fundamental challenges in civil engineering. The aim of this study is to evaluate the mechanical properties of fiber concrete containing glass powder as a replacement for 0-3 sand and basalt powder as partial cement substitutes after exposure to high temperatures. In this study, glass powder was used as 10% of the 0-3 sand and basalt powder was prepared as a replacement for 20% of the cement consumed. After 28 days of curing, the samples were exposed to temperatures of 300 and 600 degrees Celsius and subjected to compressive, tensile, flexural, electrical and water absorption tests. At temperatures of 300 and 600°C, the results showed that replacing part of the cement/sand with mineral powders at 7 days of age caused a more noticeable decrease in compressive strength than at 28 days of age, which was compensated for with the passage of time and the progress of hydration and the filling effect of fine particles. Among the modified designs, the sample of 20% basalt powder replacing cement in fiber concrete containing 0.5% fixed glass fibers showed the best mechanical performance by achieving a 28-day compressive strength of 45.9 MPa, tensile strength of 3.83 MPa, and flexural strength of 4.9 MPa, and had a very limited decrease of about 2.3 to 5.8% compared to the control sample. In the evaluation of thermal performance, increasing the temperature to 600°C led to a sharp decrease in the compressive strength of all samples due to the outflow of structural water and the formation of microcracks; However, the 20% basalt powder sample, retaining 59.9% of its initial strength of 27.5 MPa and displaying the highest percentage of residual flexural strength, provided much better thermal performance even than the control sample. In contrast, the 10% glass powder design in 0.5% glass fiber concrete as aggregate recorded the weakest thermal stability. In terms of durability parameters, the addition of glass powder and basalt made the internal structure of the concrete denser. The combined design containing 10% glass powder and 20% basalt powder in 0.5% glass fiber concrete showed the best performance in reducing water absorption to 2.4% compared to 8.4% seen in the control sample and increasing electrical resistance to 10.41 kΩ/cm, reducing permeable pores, limiting the passage of ions, and improving concrete durability.
Keywords : fiber concrete glass powder basalt powder mechanical properties high temperatures thermal durability scaling