Evaluation of the Self-Healing Performance of Asphalt Mixtures at Different Aging Levels under Microwave Heating
Evaluation of the Self-Healing Performance of Asphalt Mixtures at Different Aging Levels under Microwave Heating
Amir Kavussi1 Ali kaseb2 Omid Hajinezhad3
1) Professor, Department of Road and Transportation, Tarbiat Modares University
2) Master’s Student, Highway and Transportation Engineering
3) Master’s Student, Road and Transportation Safety Engineering, Tarbiat Modares University
IOI Code
:
ABFG-ACAGZH
Publication :
12th.international Congress on Civil Engineering, Architecture, Art and Urban Development(12icsau.ir)
Abstract :
Abstract
During the service life of asphalt pavements, the aging of bitumen characterized by increased stiffness and reduced ductility alters the mechanical performance of the asphalt mixture and renders it susceptible to cracking. In this context, microwave heating, facilitated by the inclusion of microwave-absorptive additives, has emerged as a promising technique for providing the necessary thermal energy to promote crack healing in asphalt mixtures. This study investigates the influence of varying durations of laboratory-simulated aging on the thermal response and healing performance of asphalt mixtures subjected to microwave heating. To this end, 4% steel fibers were incorporated into the asphalt mixture samples as microwave-absorptive additives. To simulate the aging process, the prepared samples were subjected to accelerated aging in a laboratory oven at 85°C for periods of 1, 3, 5, 7, and 9 days. Following these aging periods and an initial indirect tensile strength (ITS) test, the samples were exposed to microwave radiation for 120 seconds. Subsequently, after a 24-hour interval, the indirect tensile strength was re evaluated to determine the healing index. The results indicate that the initial indirect tensile strength increased as the aging duration extended up to 5 days, after which it began to decline. Furthermore, longer aging durations were associated with an enhanced thermal response of the samples to microwave heating. Regarding healing performance, samples subjected to 5 days of aging exhibited the highest healing capacity; specifically, the healing index for the sample containing steel fibers reached 73.5%. As the aging duration increased to 7 and 9 days, the healing index declined a trend attributable to increased stiffness and brittleness of the bitumen, which in turn limits its deformability. Overall, within the range of tested conditions, a 5-day laboratory aging period was identified as yielding the optimal healing performance; based on the comparisons made in this study, this corresponds to approximately 10 years of aging under actual pavement service conditions.