An overview of heat treatment parameters (intercritical annealing time and temperature, and tempering) on the mechanical properties of steel 1.1525

An overview of heat treatment parameters (intercritical annealing time and temperature, and tempering) on the mechanical properties of steel 1.1525

Abdollah Kazemi1 Mohammad Jiryaei2 Shahrouz Yousefzadeh3

1) Senior Master s Expert in Mechanical Engineering, Manufacturing and Production Orientation, Faculty of Engineering, Islamic Azad University, Aligudarz Branch, Iran
2) Senior Master s Expert in Mechanical Engineering, Manufacturing and Production Orientation, Faculty of Engineering, Islamic Azad University, Aligudarz Branch, Iran
3) Assistant Professor of Mechanical Engineering – Solid Design, Faculty of Engineering, Islamic Azad University, Aligudarz Branch, Iran

IOI Code : ACCD-ACAABZ
Publication : 10th International Conference on Applied Researches in Science & Engineering (carseconf.com)
Abstract :
    Carbon tool steel 1.1525, also known as C80W1 and W1, is used in the manufacture of cutting tools and industrial components due to its relatively high carbon content, hardenability, and reasonable cost. However, achieving high hardness and strength without a severe loss of toughness and ductility is one of the main challenges in the heat treatment of this steel. The aim of the present paper is to review the theoretical foundations and the evidence presented in the attached source regarding the role of austenitizing temperature, tempering temperature, and quenching medium on the microstructure and mechanical properties of 1.1525 steel. The methodology is a narrative and analytical review of the content of the attached thesis and the categorization of its concepts, reported background, and experimental results; therefore, the present paper does not claim to be an independent systematic review or an external verification of all sources. According to the reported data, an increase in austenitizing temperature was accompanied by an increase in yield and tensile strength, and sample F, with an austenitizing temperature of 840 °C and tempering at 280 °C, showed the highest yield strength (669 MPa) and ultimate tensile strength (1012 MPa); at the same time, elongation and impact energy decreased in this sample, with impact energy reported at approximately 7.3 J. The results of the source indicate that the selection of the heat treatment cycle should be based on a balance among strength, hardness, toughness, and ductility. Furthermore, definitive conclusions regarding the role of boiling salt water and the phases formed require more precise control of holding time, measurement of the core temperature of the part, and quantitative microstructural analysis.

Keywords : 1 1525 steel carbon tool steel austenitizing quenching tempering hardness tensile strength impact toughness microstructure