Laboratory investigation of compressive strength of self-compacting concrete mixtures with replacement of rubber instead of sand

Laboratory investigation of compressive strength of self-compacting concrete mixtures with replacement of rubber instead of sand

saeid darvishi1 farshid zarei2

1) Civil engineering student
2) Civil engineering student

IOI Code : XHFC-AZBHBG
Publication : 6th.International Conference & 7th.National Conference on Civil Engineering, Architecture, Art and Urban Design(7iccacs.ir)
Abstract :
    One of the most important properties of concrete is its compressive strength, which indicates the ability of concrete to withstand compressive loads without crushing or cracking. Irregular distribution of corroded rubber in the concrete mixture can negatively affect its quality and final properties. The purpose of this research is to investigate the compressive strength of self-compacting concrete mixtures by substituting rubber instead of sand. The method of this research is through testing and the hardened properties of self-compacting concrete in two states without heat and heated samples under different temperatures of 300, 600 and 900 degrees Celsius have been investigated. The heating of concrete samples was done at the rate of one degree centigrade per minute. The mixing scheme used in this research to achieve self-compacting concrete was according to ACI 237R-07 guidelines. In order to investigate the factors affecting the hardened properties of self-compacting concrete in concrete samples at high temperatures, in addition to using different amounts of rubber crumb, two ratios of water to cement materials and two sizes for the largest dimension of aggregates were used and the effect of each of them In the fresh state, it was checked by slump flow tests, V funnel and L-shaped box. In order to measure the compressive strength of hardened concrete, cubic samples with dimensions of 10x10x10 cm were used according to B.S 1881: Part 116 standard. Then, in order to evaluate concrete samples containing rubber crumb at the age of 90 days, compressive strength tests, ultrasonic tests, water absorption and weight reduction were performed on them. The results of this research show that increasing the ratio of water to powder materials from 0.34 to 0.39 has caused a decrease of 6.6% in the results of compressive strength. At the temperature of 20 degrees Celsius, the increase of the largest dimension of aggregate from 12.5 to 19.5 mm did not result in a significant change in the results of this test and to some extent (0.3%) it showed a compressive strength in the same mixtures, which seems to be It seems that this case is due to the better consistency of the granulation curve in the case where the largest dimension of the aggregate is 19.5 mm.

Keywords : self compacting concrete rubber corrosion compressive strength