Optimization of direct leaching of sphalerite concentrate at atmospheric pressure
Optimization of direct leaching of sphalerite concentrate at atmospheric pressure
farzad rahimi1
1) Graduated with a bachelor s degree in mining engineering, mining specialization, Yazd National University, Yazd, Iran
IOI Code
:
XKBA-AZFABA
Publication :
3rd International Conference on Recent Advances in Engineering, Innovation and Technology - Belgium(eitconf.com/3rd)
Abstract :
In this research, the optimization of direct leaching process of sphalerite concentrate from Bama mine at atmospheric pressure was investigated by surface response method. After conducting mineralogical tests and identifying the chemical composition of the sample, 13 preliminary tests were conducted on four levels in order to identify the effect of the parameters. After the initial tests, in order to perform additional tests and optimize the process, 32 tests were performed using the surface response method and the number of 5 two-level parameters, including sulfuric acid concentration, ferric ion concentration, solid-to-liquid ratio, temperature and stirring speed with Design Expert software was used. The highest recovery in the conditions of sulfuric acid concentration of 0.6 mol/liter, ferric ion concentration of 1 mol/liter, temperature of 75 degrees Celsius, solid-to-liquid ratio of 3%, stirring speed of 550 rpm in a period of 4 hours is equal to 80 The percentage was obtained. Finally, according to the analysis of the results of variance analysis, solid-liquid ratio was determined as the most effective and sulfuric acid concentration as the least effective parameters, and the most significant interaction between temperature parameters and solid-liquid ratio was obtained. The optimal conditions obtained by design expert software are equal to sulfuric acid concentration of 0.2 mol/liter, ferric ion concentration of 1 mol/liter, temperature of 89.91 degrees Celsius, solid to liquid ratio of 1%, around The stirrer was 700 rpm and the recovery was determined to be 71.71%.
Keywords : direct leaching sphalerite optimum surface response zn