Abstract :
    The aim of this study was to provide Poplar’s Wood-polymer Composite to improve the physical ‎properties and practical use in industry. In order, a sample test is done with Monomer Methyl methacrylate ‎‎with the method of filled cell saturation and then heating in the oven to be polymerized at 140 and 150 °C and times of 4 and 5 h. After providing ‎Poplar’s Wood-polymer Composite, the physical characteristics of Poplar wood (such as water adsorption, special gravity,‎ dimensional change) were analyzed. The results taken from one-way variance showed that the changes mostly ‎weren’t significant. In temperature changes, only the percentage of polymer establishment was significant and in time ‎changes no percentage was significant. In the analysis of factorial variance, the dependent effect of temperature and ‎time, the only significant was percentage of polymer establishment and water adsorption. Survey results and analysis show that all the studied physical properties including water absorption, dimensional change and specific gravity, in compare with control have improved.

Keywords : poplar physical characteristics methyl methacrylate ‎ wood polymer composite