The use of electrochemical anodized aluminum foil as a cathode current collector of lithium-ion battery

The use of electrochemical anodized aluminum foil as a cathode current collector of lithium-ion battery

Mohammad Mohsen Loghavi1 Mohsen Babaiee2 Rahim Eqra3

1) Institute of Mechanics, Iranian Space Research Center, Shiraz, Iran
2) Institute of Mechanics, Iranian Space Research Center, Shiraz, Iran
3) Institute of Mechanics, Iranian Space Research Center, Shiraz, Iran

IOI Code : XBCG-DCCCG
Publication : 13th Biennial Electrochemistry Seminar of Iran(elect13pguac.ir)
Abstract :
    The aluminum foil, used as a cathode current collector in a lithium-ion battery, plays a decisive role in battery cycle life through its ability to maintain active material on itself [1]. In this study, the surface of Al-foil was anodized by a simple electrochemical technique. Then, this modified collector was used in cathode electrode of Li-ion coin cell and compared with a bare-collector electrode. For preparing the modified collector, firstly, Al-foil (surface area of 25 cm2) was rinsed with ethanol, and then immersed in potassium hydroxide and nitric acid solutions for 10 seconds, respectively. Subsequently, this foil was placed against a cathode of stainless steel in a solution of sulfuric acid. Current of 0.8 A was set up between the cathode and the anode to perform the anodizing process. The surface morphology of bare and modified aluminum foil was investigated using scanning electron microscopy. The wettability of the surface of the collectors was analyzed by the contact angle test via Data Physics OCA 15 plays instrument. In this method, a drop of normal methylpyrrolidone solvent is placed on the foil surface, and the contact angle created between the solvent droplet and the foil surface is immediately measured [2]. Active material (LiNi0.8Co0.15Al0.05O2), conductive additive (Super PLi) and binder (Polyvinylidene fluoride) were used to prepare the cathode electrodes. In order to determine the adhesion of cathode materials to the current collector surface, the test of immersion of electrode disk in electrolyte was used. The electrolyte used in this study was a solution of 1 M LiPF6 salt in EC/DEC (1:1 v/v). To evaluate the electrochemical properties of cathode electrodes, coin cells were prepared in which lithium chips were used as anode and reference electrode, and then these cells were charged and discharged between 2.8-4.2 V at a rate of 0.5 C during 100 cycles via BTS8000 (Neware company). As shown in Fig. 1, the SEM images indicate a rough surface for anodized current collector and a relatively smooth surface for bare current collector. The results of the contact angle test indicate higher wettability of the modified aluminium foil against the bare foil. The high adhesion of active materials to the modified current collector was demonstrated through the test of electrode immersion in electrolyte. The cycleability results indicate that the modified-collector electrode has the ability to maintain a capacity of 85% in 100 cycles, but the bare-collector electrode retains only 66% of its initial capacity after 100 cycles.

Keywords : anodized battery current collector li ion surface modification cathode