Analysing the Effect of Using Plastic Waste HDPE on the Fracture Mechanism and Durability of Recycled Hot Mix Asphalt
Analysing the Effect of Using Plastic Waste HDPE on the Fracture Mechanism and Durability of Recycled Hot Mix Asphalt
Farid Sheibani Behrouz1 Shahin Shabani2 Mona Taheri3
1) Master s Student; Civil Engineering (Road and Transportation specialization); Payame Noor University, Tehran, Iran;
2) Associate Professor; Department of Civil Engineering; Payame Noor University, Tehran, Iran;
3) Assistant Professor; Department of Chemical Engineering; Payame Noor University, Tehran, Iran;
IOI Code
:
AAHE-ACZDCF
Publication :
National Conference on Civil Engineering, Design and Construction Technologies, Energy, Materials and Advanced Machinery(icaeu.ir)
Abstract :
Simultaneously returning two waste streams (reclaimed asphalt pavement and waste plastic) to hot mix asphalt is an engineering problem before it is an environmental solution, because the aged binder of the reclaimed material shifts the mixture balance from ductility towards stiffness, and the added polymer is itself a stiff material. The more important methodological problem is that most studies in this field have based their evaluation on surrogate strength indicators that do not measure the cracking dimension. This study evaluated the effect of waste high-density polyethylene on the fracture mechanism and durability of recycled hot mix asphalt using a full factorial design and performance-based criteria. Eight mixture groups were produced by combining two bases (virgin aggregate, and a mixture containing 50 percent reclaimed asphalt pavement) with four polymer levels (0, 1, 2 and 4 percent by total mixture weight, added through the dry process), while total binder content was held constant at 4.9 percent in all eight groups. Specimens were compacted with a Superpave gyratory compactor in 150 mm moulds at 100 design gyrations and evaluated with three tests: the indirect tensile asphalt cracking test at 25 °C, the semi-circular bend test at −10 °C and −17 °C, and the tensile strength ratio test. Data from 120 specimens were analysed by two-way analysis of variance and the Tukey honestly significant difference test at a five percent significance level. The results showed that adding 4 percent polymer to the recycled mixture significantly increased peak load by 76 percent, fracture energy by 19 percent and indirect tensile strength by 35 percent, and raised the tensile strength ratio to 99.2 percent; but it simultaneously shortened the displacement at failure by 39 percent, and the cracking tolerance index showed no significant improvement in any group. A significant interaction between mixture base and polymer content showed that the effect of this additive on strength is several times larger in the recycled base than in the virgin base, whereas no such difference appears in the ductility dimension. All eight groups passed the tensile strength ratio acceptance threshold by a considerable margin. The engineering conclusion is that the polymer makes the recycled mixture stronger and more durable but less ductile. A volumetric design-space analysis showed that every one percent of polymer by total mixture weight occupies about 2.5 percent of the mixture volume, so the dosage ceiling in the dry process is a volumetric constraint before it is a mechanical one: in a conventional dense gradation the dosage should stay below one percent by total mixture weight, and higher dosages require a gap gradation with a correspondingly adjusted effective binder content.
Keywords : recycled plastic hdpe fracture mechanism durability recycled hot mix asphalt